Way is the consumable you are proposing for the wps
For welder qualification consumable is major weighted parameter
Thanks and Regards
Lakshmankumar B
9440031459
Sent from my iPhone
Dear Gentlemen,--I have to qualify welder with base material in my hand is P-1 to P-1, but but actual WPS done on P-1 to P-43 base material. May i proceed to qualify the welder based on this WPS?Thanks in advance.Regards,Venkkatesh Gopalakrishnan.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Comments