Sunday, October 8, 2017

[MW:26888] RE: 26879] Weld overlay PD5500

Hello Abhishek,

 

Existing ASME Sec-IX qualified PQR's will not meet the requirements of ISO-15614-7(2007 version).Please see the extracts on the dimension of test coupons and various testing requirements.

Note the footnotes are the fine prints.

 

If your organization is in  the business of  fabricating pressure vessels to PD 5500, it's advisable to have separate set of  PQR's qualified to ISO-15614-7 .

 

In fact one PQR may support many required Welding Procedure Specifications  if all the testing are done with good prior thinking.

 

Thanks.

 

P.Goswami.P.Eng, IWE.

Welding & Metallurgical Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@quickclic.net,pradip.goswami@gmail.com

 

 

 

-----Original Message-----

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of ABHISHEK SINGH

Sent: October 7, 2017 7:58 AM

To: Materials & Welding <materials-welding@googlegroups.com>

Subject: [MW:26879] Weld overlay PD5500

 

Dear Experts,

 

In my Job construction code is PD5500. Can I use Overlay  PQR qualified as per ASME Sec. IX instead of EN15614-7??

 

Regards

Abhishek Singh

 

--

https://materials-welding.blogspot.com/

https://www.linkedin.com/groups/122787

---

You received this message because you are subscribed to the Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

Visit this group at https://groups.google.com/group/materials-welding.

For more options, visit https://groups.google.com/d/optout.


Virus-free. www.avg.com

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...