Supplementary requirements shall not apply unless specified in the purchase order. if so it will be specified in MTC (if it is directly from the mill), else check testing is an acceptable alternative.

On 5 October 2017 at 08:00, chiluka venkatramulu <ramuluchiluka@gmail.com> wrote:
Dear Experts,
Pl clarify the S5 Supplementary requirements for SA-516 Gr 70. Is it reflect in MTC or it will be tested separately after receiving material at work shop.

Thanks in advance,
Venkat



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...