Monday, October 16, 2017

Re: [MW:26913] using of ER308 filer.

Since it is dissimilar joints, u can match with 304 or 316L. 308 is not bad selection, ref B31,1 for further

On 16-Oct-2017 7:55 am, "José Juan Jiménez Alejandro" <jjjimeneza@gmail.com> wrote:
Boxbe This message is eligible for Automatic Cleanup! (jjjimeneza@gmail.com) Add cleanup rule | More info

And your wps?

El 15 oct. 2017 9:17 PM, "'sangram routray' via Materials & Welding" <materials-welding@googlegroups.com> escribió:
Dear group members ;
our sub-contractor welded one joint  304 PIPE to 316L valve by ER308 filler but client said its not acceptable.
can some one help me regarding above mater .
is it Acceptable or not? 
Answerd with some code or standard reference. 
 
Thanks & Regards

Sangramkeshari Routaray
Welding inspector

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...