in which specification it is mention about thickness > 6mm ,
On Saturday, 10 September 2011 19:15:33 UTC+4, Harish wrote:
-- On Saturday, 10 September 2011 19:15:33 UTC+4, Harish wrote:
Impact test is mandatory for t>6mm, if the material is going for low temperature service.2011/9/10 arvinda shan <arvin...@gmail.com>
--Dear Experts,For crosshead installation in jetty project, the following materials (37mm) are used.Road way - S355JO
Crosshead - S355JR & S275JR
Pipe track - S355JR
As per European structural steel standard EN10025 , for JR grade, Longitudinal charpy V-notch impacts 27J @20 degrees and for JO grade, Longitudinal charpy V-notch impacts 27J @ 0 degrees.
We received materials mill certificates w/o impact test.
My question is whether impact is mandatory for above grades or any criteria of thickness as per EN10025? Please mention with reference codes.
Your valuable suggestions are appreciated.
Regards
arvinda
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--regards,Harish.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Comments