Re: [MW:26792] IS IGC test Required ?

Any welding involved.
 
Thanks & Regards
J.Gerald Jayakumar
0091-9344954677



From: Aakash <harenathjha@gmail.com>
To: Materials & Welding <materials-welding@googlegroups.com>
Sent: Wednesday, September 6, 2017 10:03 AM
Subject: [MW:26790] IS IGC test Required ?

Hello Expert,
Following are the situation,
Material, SA 312 Typ 304 L (Carbon content is >= 0.03 %)
Joining process :- Welding by GTAW process
Service Temprature -90 Degree (MAximum)
Pressure - 7kg/cm2 (maximum)

Service fluid :- Water,

Is IGC Test ( ASTM 262) is required to be carried out ?

As per my understanding, it is not required.

You please give your advice

Regards
HNJ
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...