Impact test is mandatory whenever ,there is lower service temperature,Grades you have specified might be impact tested by the mill,coz these grades are generally used for low service temperature.

On Saturday, September 10, 2011 at 1:10:54 PM UTC+5:30, arvinda wrote:
Dear Experts,
 
For crosshead installation in jetty project, the following materials (37mm) are used.
 

Road way            - S355JO

Crosshead           - S355JR & S275JR

Pipe track            - S355JR

 

As per European structural steel standard EN10025 , for JR grade, Longitudinal charpy V-notch impacts 27J @20 degrees and for JO grade, Longitudinal charpy V-notch impacts 27J @ 0 degrees.

 

We received materials mill certificates w/o impact test.

 

My question is whether impact is mandatory for above grades or any criteria of thickness as per EN10025? Please mention with reference codes.

 

Your valuable suggestions are appreciated.

 

Regards

 

arvinda

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...