Thursday, September 28, 2017

Re: [MW:26843] SR equirement for Heads

As per code it is not reqd but EIL spec says.
What to follow


On 28 Sep 2017 07:47, "Vijay Patre" <vijay.patre09@gmail.com> wrote:
as per recommended practice sr shall be followed for 16 & 20mm thick head, for others pls check fibre elongation...

however, as per code all cold formed dish end shall be heat treated.

On Sep 26, 2017 9:19 PM, "Pankaj Kolhe" <pankaj.kolhe15@gmail.com> wrote:
Dear Experts,

AS per IL spec.all cold formed heads need to be stress relieved.
we have 6mm,10mm,12mm,16mm & 20 mm thk dish end in our job.

so my question is shall i do SR for all thickness dish end or how to proceed.

MOC 516-70


pankaj

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...