find the welder qualification Requirements as follows
Welding Procedure and Welder Qualification coupon SET-UP:
Welder Qualification:
A welder qualified on pipe having an OD of greater than or equal to 12.750 in. (323.9 mm) should be qualified for all pipe diameters. A welder who has an existing Unlimited Thickness qualification to ASME-IX and an in-service qualification as per Fig. above to the 2 pipe thickness as stated in the table below, should be qualified as an in-service branch or sleeve welder for Horizontal Pipe positions, all diameters, and all wall thicknesses.
Hot Tap Welder Performance Coupon Requirement for Qualifying 2 Welders | ||
ITEM DESCRIPTION | CARRIER PIPE | SPLIT SLEEVE |
T upon 19.1mm | 12" SCH 40 (10.3mm) X 600mm LONG | 14" SCH – XS (12.07mm) X 200mm LONG |
T > 19.1mm | 14" SCH – 100 (23.83mm) X 200mm LONG | |
Note:If the welders Qualified on thickness more than 19.1mm, will qualified to weld unlimited thickness can be Utilized for future projects
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Comments