Monday, September 11, 2017

[MW:26809] RE: 26807] Weld JFE EH500

Hi Emilio,

Please see the catalogue as below. If may have all the relevant information including the recommended welding consumables.

 

Thanks.

 

P.Goswami.P.Eng, IWE.

 

http://www.totalsteel.com.au/downloads/JFE-EH-Catalogue.pdf

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Emilio Cerato
Sent: September 10, 2017 11:44 AM
To: Material Welding <materials-welding@googlegroups.com>
Subject: [MW:26807] Weld JFE EH500

 

Dear,
 I have to weld a material identified as JFE EH500.

 

According to the supplier's catalog recommend using ER70S3 or ER80S3 wire, 
controlling preheating and heat supplied.
 
This work is for a mining company, in which I have no manufacturing standard
The question is how do I qualify the procedure?
 
What is the resistance of the tensile test?
With what punch diameter should I make the folds?
Is it advisable to use AWS B2.1?
 
I appreciate your comments.


Thanks.


Emilio Cerato
 
 

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.




AVG logo

This email has been checked for viruses by AVG antivirus software.
www.avg.com


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...