[MW:26828] SA 335 P91 preheat pwht conditions and variables

Dear friends,
Could anyone please guide me with codes and standards with respect to welding of SA 335 P91 pipes for high pressure and temperature boiler lines,

Looking forward for your contribution.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS