[MW:26794] ASTM A106 grade B pipe

is impact test required for ASTM A106 grade B pipes??? and is yes what will be the testing temperature?

Vijay

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

1 comment:

mansukh said...

no require for A106 grade B

Mansukh Satashiya
| ASNT NDT Level III RT UT MPT PT| Welding Inspector CSWIP 3.1 | Lead Auditor ISO 9001:2008
T +91 7227039190 | WhattsApp 9726371394
E satashiyam@yahoo.co.in;satashiyam@gmail.com

Re: [MW:35686] HDPE WPS