Hi all, 

Normally for sour service application , brand is an essential variable only for Nickel base and duplex consumable  . Trade name may vary and can be changed as long as same F number and A number is matching need to make one additional supplement chemical analysis and you may proceed  if client agrees.
This is my suggestion only.

P.NEILASHKUMAR 
Sent from my iPad
MOB : 966 551094590
             +91 9952110791

On 31-Aug-2017, at 10:35 AM, PREM SHANKARDUTT NAUTIYAL <prem_nautiyal@rediffmail.com> wrote:


ESAB is the welding consumable manufacturer name whereas OK TIGROD 16.30 is the Brand Name.
Hence in this case the change in brand name is an essential variable.

Regards

Prem Nautiyal


On Wed, 30 Aug 2017 19:38:26 +0530 "'james gerald' via Materials & Welding" wrote
> It is change from OK TIGROD16.30 to OK TIGROD16.10, For Sour Service as defined by the Materials Engineer with certain PPM & PH of H2S, the above change is an essential variable.

Thanks & RegardsJ.Gerald Jayakumar0091-9344954677

From: Umang Parikh
To: materials-welding@googlegroups.com
Sent: Wednesday, August 30, 2017 11:34 AM
Subject: [MW:26764] Regarding brand name of welding consumable.

Dear friends,Please clarify below point.( This is one of the project spec.)
"Any change in brand name of the filler metal if the service is sour"
What is the meaning of this sentence.Is it mean to say change in the company name or company product name.i.e ESAB TO ESAB orits product OK TIGROD 16.30 TO OK TIGROD 16.10.
Can we make WPS of 316L with supporting PQR 304L if the above clause is essential variable as per project spec.
Appreciate to have views on above point ASAP



--

https://materials-welding.blogspot.com/

https://www.linkedin.com/groups/122787

---

You received this message because you are subscribed to the Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

Visit this group at https://groups.google.com/group/materials-welding.

For more options, visit https://groups.google.com/d/optout.






--
>
https://materials-welding.blogspot.com/
>
https://www.linkedin.com/groups/122787
>
---
>
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
>
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
>
Visit this group at https://groups.google.com/group/materials-welding.
>
For more options, visit https://groups.google.com/d/optout.
>


PREM S NAUTIYAL
CELL : 9769316004

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...