[MW:26694] Re: Longitudinal Weld overlay

I have come across situation that even for 250 mm nozzle ID weldoverlay has been in longitudinal direction and approved by Korean client.

Standard good practice is to apply weld overlay in circumferential direction. However in case of small diameter nozzles is to deposit weld overlay in the longitudinal direction.

This is to avoid the overheating (too high inter pass temperature) which should occur in case the weld overlay is applied in the circumferential direction.

Regards
Bharathi

On Thursday, December 8, 2016 at 8:46:44 PM UTC+9, ABHISHEK SINGH wrote:
Dear experts,
      Anyone know why some of the client not allowed for overlay in longitudinal direction in nozzle I. D, PIPE I.D,Elbow I.D. Is there are any technical reason??

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...