Dear Friends
A column is going to be fabricated as per ASME Sec VIII Div.1
The shell plate material is SA 516Gr.70 (14mm thk) + SS 410S (3.5 mm thk) Roll Bonded clad plate.
Client spec. mentions undiluted chemistry of SS 410S at height of 3mm for the roll bonded clad plate.
My doubt is whether plate manufacturer can achieve this stringent requirement ?
PREM S NAUTIYAL
CELL : 9769316004
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment