Wednesday, August 30, 2017

[MW:26764] Regarding brand name of welding consumable.

Dear friends,
Please clarify below point.( This is one of the project spec.)

"Any change in brand name of the filler metal if the service is sour"

What is the meaning of this sentence.
Is it mean to say change in the company name or company product name.
i.e ESAB TO ESAB or
its product OK TIGROD 16.30 TO OK TIGROD 16.10.

Can we make WPS of 316L with supporting PQR 304L if the above clause is essential variable as per project spec.

Appreciate to have views on above point ASAP 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...