Re: [MW:26725] ER 347 Vs E347 CVN impact values

There is No IGC or Ferrite number requirements.

However the welding consumable manufacturer have opined that due to ferrite content in SMAW process they cannot guarantee impact at such low temperatures at minus 196 degree Ceclius.

On Thu, 17 Aug 2017 11:59:26 +0530 "'james gerald' via Materials & Welding" wrote
> I suppose there is some problem with the selection of material, SS 321/347, which contains Titanium / Niobium which are Ferrite formers and for -196degC service why do you need IGC control. Try 304LThanks & RegardsJ.Gerald Jayakumar0091-9344954677

From: Pandithan
To: PREM SHANKARDUTT NAUTIYAL
Cc: materials_welding
Sent: Thursday, August 17, 2017 10:12 AM
Subject: Re: [MW:26723] ER 347 Vs E347 CVN impact values

For TIG, try with ER321
On 16-Aug-2017 11:54 PM, PREM SHANKARDUTT NAUTIYAL wrote:






This message is eligible for Automatic Cleanup! (prem_nautiyal@rediffmail.com)
Add cleanup rule
| More info






Dear friends

A vessel will be fabricated as per EN 13445 - 2014 edition.

As per contract impact test is mandatory at minus 196 degree Celsius with Min. Impact value of 40J.

Base material is SS 321.
Thickness ranging from 10mm to 20mm.

Two separate PQR are being conducted as per EN ISO 15614-1.

1. Complete TIG with ER 347 with controlled heat input less than 1KJ/mm
PQR coupon thickness was 14mm.
= impact values are coming on weld avg 30J - Failed.
HAZ = @ 55 J and passing.

Now trying PQR with other brand.

2. Complete MMAW = E 347 - Here consumable manufacturer in India have regretted impact properties at minus 196 degree Celsius.

Both TIG and MMAW consumables are having @ 8 FN.

Then why MMAW Consumable manufacturer in India have regretted impact properties at minus 196 degrees Celsius for MMAW process E347 ?

Difficult to understand !

Regards

Prem Nautiyal
IWE



PREM S NAUTIYAL
CELL : 9769316004




--

https://materials-welding.blogspot.com/

https://www.linkedin.com/groups/122787

---

You received this message because you are subscribed to the Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

Visit this group at https://groups.google.com/group/materials-welding.

For more options, visit https://groups.google.com/d/optout.





--

https://materials-welding.blogspot.com/

https://www.linkedin.com/groups/122787

---

You received this message because you are subscribed to the Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

Visit this group at https://groups.google.com/group/materials-welding.

For more options, visit https://groups.google.com/d/optout.






--
>
https://materials-welding.blogspot.com/
>
https://www.linkedin.com/groups/122787
>
---
>
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
>
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
>
Visit this group at https://groups.google.com/group/materials-welding.
>
For more options, visit https://groups.google.com/d/optout.
>


PREM S NAUTIYAL
CELL : 9769316004

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...