Thursday, August 17, 2017

Re: [MW:26725] ER 347 Vs E347 CVN impact values


Mostly i have seen SS 321 welded with 347.

Can ER 321 give impact properties at minus 196 degree celcius ?

On Thu, 17 Aug 2017 11:42:30 +0530 Pandithan wrote
>For TIG, try with ER321
On 16-Aug-2017 11:54 PM, PREM SHANKARDUTT NAUTIYAL wrote:





This message is eligible for Automatic Cleanup! (prem_nautiyal@rediffmail.com)
Add cleanup rule
| More info

>




Dear friends
>
>A vessel will be fabricated as per EN 13445 - 2014 edition.
>
>As per contract impact test is mandatory at minus 196 degree Celsius with Min. Impact value of 40J.
>
>Base material is SS 321.
>Thickness ranging from 10mm to 20mm.
>
>Two separate PQR are being conducted as per EN ISO 15614-1.
>
>1. Complete TIG with ER 347 with controlled heat input less than 1KJ/mm
>PQR coupon thickness was 14mm.
> = impact values are coming on weld avg 30J - Failed.
>HAZ = @ 55 J and passing.
>
>Now trying PQR with other brand.
>
>2. Complete MMAW = E 347 - Here consumable manufacturer in India have regretted impact properties at minus 196 degree Celsius.
>
>Both TIG and MMAW consumables are having @ 8 FN.
>
>Then why MMAW Consumable manufacturer in India have regretted impact properties at minus 196 degrees Celsius for MMAW process E347 ?
>
>Difficult to understand !
>
>Regards
>
>Prem Nautiyal
>IWE
>
>
>
>PREM S NAUTIYAL
>CELL : 9769316004
>



--
>
https://materials-welding.blogspot.com/
>
https://www.linkedin.com/groups/122787
>
---
>
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
>
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
>
Visit this group at https://groups.google.com/group/materials-welding.
>
For more options, visit https://groups.google.com/d/optout.
>




--
>
https://materials-welding.blogspot.com/
>
https://www.linkedin.com/groups/122787
>
---
>
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
>
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
>
Visit this group at https://groups.google.com/group/materials-welding.
>
For more options, visit https://groups.google.com/d/optout.
>


PREM S NAUTIYAL
CELL : 9769316004

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...