Dear Mr.Rameez

Gate valves are Bi -direction valve's hence flowdirection not important.flowdirection to be ensured for globe valve's and check valve only.


On Tue, Aug 22, 2017 at 7:58, Rameez khan RK
<rk.rameezkhan21@gmail.com> wrote:
Dear Expat,
                       I have a question regarding gate valve flow direction. if the direction change during fit up then what type of problem facing can any one tell me regarding this issue. 



Thanking you

Rameez khan 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...