Dear all experts.
 
Pl need feedback and further in depth understanding on the following points:
 
Case1:                                                         
one metal from P No. 3 to any
metal from P No. 3 does not qualify P No. 1 to P No. 1
Plate_P_1_1_Not
 
Case 2:
It qualifies one metal from P No. 4 to any
metal from P No. 4, 3 or 1. but does not qualify P No. 3 to P No. 3 or P No. 1 to P No.1
Plate_P_3_1_3 or 1_Not
 
I would much appreciate if someone give more details regarding, grouping for base metals with weld metals, for similar and dissimilar metals.
 
Thanks
 
Razz Khan
Welding Inspector
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...