Hi MNK,
What were the temperature/time parameters of the :
1. Weld preheat heat treatment (PHT) and interpass?
2. The post weld dehydrogenation heat treatment (DHT)?
3. The post DHT cooling?
4. The post weld heat treatment (PWHT)?
Regards,
DT
-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of mmm
Sent: Friday, August 04, 2017 6:43 AM
To: Materials & Welding
Subject: [MW:26698] Welding of F91 material
Seal weld joint between bonnet and body
1)Weld deposit thickness is 8mm.
2)design code- API-602
3)Electrode - E9015-B91
4)base material for bonnet and valve
body- SA 182 Gr F91
5)hardness of the weld joint is 300 BHN.
Dear experts
a)Please let me know what are method to reduce the Hardness of the weld joint?
b) is this electrode is correct or not please specify if its wrong
Thank you.
MNK
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment