Dear sir,

Do you have any brand name or any specification sheet for this product then please inform me on asgandhi.90@gmail.com

Regards,
Ankit

On Tuesday, 2 August 2016 11:41:33 UTC+5:30, manjunath madiwalar wrote:
Dear Ankit,
You can wrap gum pu sheet during fabrication to avoid contamination once fully fabricated take out sheet and passivate the whole equipment. Which is cost effective also most of industry follow the same. Gum PU rolls are available in market.
Regards.
Manjunath. T Madiwalar




On Monday, August 1, 2016, Ankit Gandhi <asgan...@gmail.com> wrote:
> Dear sir,
> Can you suggest any material or coating[in INDIA] on Stainless steel for avoiding contamination during fabrication.
> Regards,
> Ankit Gandhi
>
> --
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
> To post to this group, send email to material...@googlegroups.com.
> To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ab8289e0-5322-44ff-abbc-eac839165863%40googlegroups.com.
> For more options, visit https://groups.google.com/d/optout.
>

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b41713d8-46ea-4b5d-acce-d14f3028140e%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...