In the UK we call them gas flats. Please see the comments in the article from TWI - The Welding Institute.

 

http://www.twi-global.com/technical-knowledge/job-knowledge/submerged-arc-welding-consumables-part-1-087/

 

Alan Denney

AKD Materials Consulting Ltd

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Nilesh Pathare
Sent: 11 September 2016 17:11
To: materials-welding@googlegroups.com
Subject: Re: [MW:25370] Saw Welding pokemarks.

 

Dear Dinesh,
We have also experienced the pokemarks on SAW beads.
We analysed the reason due to powdery flux. Due fine powder in flux the gases are not able to escape prior to solidification. If you observe the slag you will find the ditches on slag surface.
1. Pokemarks on filling passes are not a problem. Ensure  welder is cleaning the bead thoroughly prior to deposit next pass.
2. For final pass ask the welder to pass the baked flux through the mesh and use only granular flux for final pass.
3. Reduce the amount of flux heap on weld bead. Pls. Use optimum quantity of flux to submerge the arc.

Regards,
Nilesh Pathare.

 

On 11-Sep-2016 6:20 PM, "Dinesh Somwanshi" <som.din@gmail.com> wrote:

Dear sir,

We are observing an pokemarks on Saw welding weld bead continuously.

The flux has used by baking.

Pls guide.

Dinesh V Somwanshi
Api 570, Cswip 3.1,Bgas 2
Authorised Certified Piping, Welding, Painting Inspector.
00919881344135

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAELgRrV4EZNPkvz-JBo28_a39f9k3T-tXf07YFRGEjFL%2BqrxLQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJ%3DxBSPqCUEZdC1-3XYwz2mxPy2QYsdK2otngQ_7SSH6mqmZ7g%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...