Need  experts advice, below detail based on old project ref


Temp for Normalizing steel - 600 to 630 degree C
Holding time - 3 to 4 hrs for thickness 15mm to 40 mm
No of cycle - 1



 


On Sat, Sep 17, 2016 at 11:19 AM, George Dilintas <dilintas@gmail.com> wrote:
you can use that one for Pno 1 material

2016-09-17 10:07 GMT+03:00 senthil thandesh <thandesh@gmail.com>:

Dear Experts,


Good Morning,


We are having our own project to build an offshore jacket for a depth of 15 to 20 meter water depth. For this project we are in the stage to order the material (PIPE) from the Steel Mill. In order to start the process the mill is asking for the SPEC of PWHT. So can anyone able confirm what should be the Holding temp / time / No of cycle / Stress relieving cycle required for PWHT.


Sl.No

Material Size

Grade

Remark

1

24" Pipe x 25mm wall thick

API 5L Gr.X52N PSL2

Normalizing Steel

2

30" Pipe x 30 mm wall thick

API 2H GR.50 +(Z35)

Normalizing Steel

3

20" Pipe x  25mm wall thick

API 5L Gr.X52M PSL2

TMCP Steel

 

 


Regards

Thandesh

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABatnw_-jRk6uM_CiFVFgT5YQHSQM1FuWRsV6kzykJPWhUVQeQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40AbqQyfQSbN_fys9W1cjjv%3D4tTTyoHroQEoiXu%2BXkbsvg%40mail.gmail.com.

For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKtNfd%2B70cwsa%2B_dSA9uCv%3DG2RSpDngO8Bgm2ktWVokPQafSdg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...