[MW:25376] Welding vessel saddles after PWHT

A 100 mm thick and 2.5 meter diameter approximately 10 meter long Carbon steel vessel is being proposed to be PWHT'd with welded wrapper plates on it at saddle locations, so that the saddles may be welded on these wrapper plates after PWHT. This will facilitate turning the vessel on its axis on the manipulator to do extensive internal work involving austenitic SS. Request to share similar experience and precautions to be exercised, so that welding the saddles after PWHT on the wrappers do not induce significant stresses on the vessel. Also references in ASME code or other international codes that allow saddles to be welded similarly after PWHT would be useful.


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b119b560-dd81-4ca5-9d15-1861c9e80971%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...