Respected members,
One of site has non PWHT carbon steel and stainless steel pressure vessels. As they are undergoing some repair, overseas engineer suggested PWHT on repaired portion for relieving the stress and to deal with HAZ.
Doing local PWHT imposed a question that during manufacturing the WPS PQR and the welding electrode employed was okay for non PWHT job. Doing the local PWHT would necessitate revised WPS PQR and the electrode this can't be done as circ. seam is covering portion of repair. Thus we are in dilemma as to what is the way out.
Being week off I request welding and code expert to suggest their opinion.
Thank you all.
Kind Regards,
Vinod Bhatt
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/55C1BFCE-5336-4DB5-8658-912DC5E1DD42%40gmail.com.
For more options, visit https://groups.google.com/d/optout.
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment