Re: [MW:25402] Welding of UNS S 31254

The below filler wire recommended

 

ERNiCrMo-3

 

Thanks & Regards,

Mohd. Azam

Doha-Qatar



On Thu, Sep 15, 2016 at 2:23 PM, 'prem_nautiyal26' via Materials & Welding <materials-welding@googlegroups.com> wrote:

Can anyone suggest correct tig filler wire for welding of
A 182 F44 : UNS NO. S 31254

Please suggest only TIG welding consumable classified in ASME SEC  II C.

Unlisted filler wires are not acceptable to  client which is a long procedure.

Job thickness is less than 10mm.

Design temp is 85 degree Celsius

Code of construction is ASME B31.3


Regards

Prem Nautiyal 


Sent from my Samsung Galaxy smartphone.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/jkcdogkbdqjevauea98gshkm.1473938592172%40email.android.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABD%2BRXSneMSeM7Y28kyh7F%2BdEdp30LWCiqWN_JKL91dYf6-%3Dsw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...