Re: [MW:25443] 6GR Procedure Qualification - Does it cover CJP Butt Joints during production - WPS and NOT WELDER

Hi, Shashank,
Thanks for your feed back.

Do you mind sharing the code reference that permits me to do it.

I am  just referring to Table 4.1 AWS D1.1 2010 Ed. note d, which takes me to 3.12 and 3.13 and then again to 4.10, 4.13.1 and 4.13.2 and 4.13.4

Appreciate your thoughts on this,

regards
rudolf



From: 'Shashank Vagal' via Materials & Welding <materials-welding@googlegroups.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Friday, 23 September 2016, 11:19
Subject: Re: [MW:25442] 6GR Procedure Qualification - Does it cover CJP Butt Joints during production - WPS and NOT WELDER

Yes to all
 

Yours Truly,
Shashank C VAGAL




From: rudolf <rudolf.jude@gmail.com>
To: Materials & Welding <materials-welding@googlegroups.com>
Sent: Thursday, 22 September 2016 9:11 PM
Subject: [MW:25441] 6GR Procedure Qualification - Does it cover CJP Butt Joints during production - WPS and NOT WELDER

Dear folks,

I have a procedure which was qualified, tested and accepted as follows.

1. Position of Test - 6GR
2. Pipe Used 6" Sch 120 and XXS
3. Process - FCAW
4. CJP as per sketch 4.25 CJP without any backing or backgouging.


Query.

Assuming that the welder is qualified, all other things are within control, thickness, etc etc,

1. Can I weld a Plate to Plate in CJP Butt Joint which does not have access to back gouging or back welding.

2. Can I have either a Single V or Single Bevel

3. Can I use ceramic backing


Appreciate your advise,

Regards
Rudolf
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/65931c1d-77ee-4460-be89-3a55b709fdd1%40googlegroups.com?utm_medium=email&utm_source=footer.
For more options, visit https://groups.google.com/d/optout.


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/852266082.2795260.1474600770523%40mail.yahoo.com?utm_medium=email&utm_source=footer.
For more options, visit https://groups.google.com/d/optout.


No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...