pls hlep us confirm whether we need apply PWHT for every girth weld according to your experience.
pipe :API 5 L X60 HIC resistant pipe
welding method: CRC automatic
pipeline diameter and thickness:20inch 0.4inch(10MM)
medium:sour condensate 
pressure:960psi
pipeline distance:164km between two gas plant in saudi (safaniya plant to berris gas plant)
client:saudi aramco

CNPC daqing saudi 
QAQC


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f49f77aa-d202-4cc2-91c7-b5f1f828afcd%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...