On Tuesday, September 1, 2015 at 2:12:11 PM UTC+5:30, Mohd Siraj wrote:
Dear all,

As old ASME B31.3-2012  we know it was above 19mm req pwht,

now i read ASME B31.3-2014,little confused me with pwht exemption and pwht requirements and control thickenss 331.1.3?

q1- what is thik req for pwht for P1 as per b31.3 2014 ?

q2 : for P1,mentioned more than 25mm thk and 95C preheat exemption from pwht so less than 25mm not require pwht ?

 

Dear All Remember now  as per new B 31.3 now this is clear no PWHT is required if Preheat is carried out at temp.-95 Degree centigrade.

But remember one more thing if during pipe welding if inter pass could not be maintained and it have been postponed for next day then again the required temp. for welding have to be maintained. 
    
    but in case any drawing or specifically any client demands for it then it's between purchaser and manufacturer

   Animesh Srivastava 
9726304200
Linde Engineering India Pvt Ltd.

regards,
9726304200

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7c0dcb99-1044-4def-8ef7-3e792b89b6f1%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...