Re: [MW:25401] Welding of UNS S 31254

pl. refer @  https://groups.google.com/forum/#!topic/materials-welding/6VwG0H2EAPE
  • AWS A5.14/ASME SFA-5.14: ERNiCrMo-3

On 15 September 2016 at 15:23, 'prem_nautiyal26' via Materials & Welding <materials-welding@googlegroups.com> wrote:

Can anyone suggest correct tig filler wire for welding of
A 182 F44 : UNS NO. S 31254

Please suggest only TIG welding consumable classified in ASME SEC  II C.

Unlisted filler wires are not acceptable to  client which is a long procedure.

Job thickness is less than 10mm.

Design temp is 85 degree Celsius

Code of construction is ASME B31.3


Regards

Prem Nautiyal 



--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVub%3Do6-GYDjfrmMk1ACFP-biiRPxJa%2BLuuWQcLmw6Ucg0uQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...