Mr Winarko,
Please share the approved GAD from the Client to clarify further.
Hydro test is proof test, can not be waived off unless Client agrees. Require also calibration of settled liquid on the bottom plate slope.
Regards
Govin
On 13 Oct 2015 16:40, "pras ari" <alhanif.pras@gmail.com> wrote:
-- --WinarkoThanks & RegardsIs any method for substitute leak test? may be NDT or pneumatic test?Dear Sir,Please advise me about leak test (hydro-test) of HSD Fuel Tank, I have 2 (two) tank with capacity 1400 KL, We will held Leak test but but site condition and around very difficult to get water as much as 2800 kilo liters.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMoAFwrSgBgmU-%3DZKEuaK_YigrM5eBnzrYfTHsyrm%2BUvMSuYcg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANiuf9fUyqGvRsLezKx9%2BOFPNsK8btCKzGb%3DcW_tofD3HZe3SA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Comments