Re: [MW:23800] Vessel Design Temperature Change

Hi

Please revise the design documents and get it approved by ASME AI & by Client as well.
If already applied for NBR, revise and resubmit for registration again (including the changes).

Regards
P
Govindan

On 24 Oct 2015 12:27, <george.dilintas@gr.bureauveritas.com> wrote:
National Board Inspection Code part 3

Sent from my BlackBerry 10 smartphone.
From: Praphulla Phirke
Sent: Σάββατο, 24 Οκτωβρίου 2015 - 10:38
Subject: Re: [MW:23795] Vessel Design Temperature Change

Dear Sir
Thanks a lot.. Do you suggest some code reference ? The manufacture demanding us the code reference .


Warm Regards
Praphulla
Sent from my iPhone

On 23-Oct-2015, at 14:01, george.dilintas@gr.bureauveritas.com wrote:

Get in touch with a R stamp holder and apply for rerating/alteration

Sent from my BlackBerry 10 smartphone.
From: Praphulla Phirke
Sent: Παρασκευή, 23 Οκτωβρίου 2015 - 11:11
To: Materials-Welding
Subject: [MW:23779] Vessel Design Temperature Change


Dear All,

I have situation where Air Receiver Vessel made of SS 316  designed as per ASME SEC VIII DIV 1 U stamped shipped to site but not yet installed. The vessel is stored on warehouse in packed condition.

 

The Present design temperature is 70°C which need to be changed to 85°C.

 

Can you please suggest which are steps we have to take ? Any code reference for recertification ?


 

Regards

Praphulla

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/341D89B8-0E22-4517-AE8D-5DD65D81A0F5%40gmail.com.
For more options, visit https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/OF0493CB18.83F8C0F7-ONC1257EE7.002ED059-1445589080487%40LocalDomain.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/005D443A-605C-46D2-964D-E617E589896B%40gmail.com.
For more options, visit https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/OF626850A7.3C2D53AF-ONC1257EE8.002DBDFB-1445674777932%40LocalDomain.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANiuf9fP714Sw%3D5v1EZy6P2m1bDg-QivOTSL-4RN1S7YtkdxGw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...