Dear Suleman,

You've to qualify Full and partial weld repair qualification with respect to welding process / pipe material .
jijilal k.m.


K.M. JIJILAL


On 23 October 2015 at 01:05, waqas suleman <waqas.suleman@gmail.com> wrote:
Dear Members,

We qualified Welding Procedure on API 1104, now our Client is demanding Weld Repair Procedure Qualification.
In scope Weld Repair Procedure Qualification is not mentioned.
I need expert judgement that is it mandatory to qualify Weld Repair Procedure for each welding procedure in API 1104.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKhANKhXe8wcUM8B4nReA8KTi%3DQAW%3DyQBZMdSz%2BToYK3hgpiyA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHmEnHgrakpqdOmg9G4J-LuXGN5%3DpQ4A5fL-DKzTudaWY0F1zg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...