Re: [MW:23744] MT before or after PWHT?

As a good engineering practice and Final product (After PWHT) shall be carried out MT 


Thanks 

Azam


On Mon, Oct 19, 2015 at 4:41 AM, Urdiansyah <urdiansyah@gmail.com> wrote:

Dear Expert,

 

Currently I work at fabricator of Pressure vessel and Heat exchanger,

During Renewal ASME, AI question about MT shall be done before or after PWHT ?

Kindly  advice for this matter

 

Thank you for answered,

 

Best Regards,

Urdiansyah

Engineering PIC

PT.Daekyung Indah Heavy Industry

Cilegon Plant :

Jl. Australia II Kav. K1 Kawasan Industri (KIEC)

Cilegon 42443, Banten - INDONESIA 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4c4f5ad7-fc11-4d20-a7c3-0ac84044a3b2%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABD%2BRXTBgoSyTmE97dnog7wcF2AD8reonNJPsDSzWx2OzHR49w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...