Monday, October 19, 2015

RE: [MW:23756] MT before or after PWHT?

Below information can be found on the National Board website.

 

http://www.nationalboard.org/index.aspx?pageID=164&ID=377

 

 

Advantages and Disadvantages of Using Magnetic Particle Examination

 

Advantages:

  • Can detect both surface and near-surface indications. 
     
  • Surface preparation is not as critical compared to other NDE methods. Most surface contaminants will not hinder detection of a discontinuity.
     
  • A relatively fast method of examination.
     
  • Indications are visible directly on the surface.
     
  • Low-cost compared to many other NDE methods.
     
  • A portable NDE method, especially when used with battery-powered yoke equipment.
     
  • Post-cleaning generally not necessary.
     
  • A relatively safe technique; materials generally not combustible or hazardous.
     
  • Indications can show relative size and shape of the discontinuity.
     
  • Easy to use and requires minimal amount of training.

 

 

Jim Price | Welding Engineer, CWI

Direct:  320.7463439 | Fax: 417-862-5564

jimprice@polarcorp.com

 

 

 

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Tadic, Miroslav
Sent: Monday, October 19, 2015 11:00 AM
To: materials-welding@googlegroups.com
Subject: RE: [MW:23752] MT before or after PWHT?

 

Considering money in END final costs, and that MT is relativity cheap, you could use MT before and after PWHT

 

So, both examination can help you to verify any indication

 

That's my recommendation and in your place, I schedule END in that way

 

Best regards

 

Miroslav Tadic
Integrity Enginner
CEE
Gerencia de Producción - Mantenimiento
YPFB Chaco S.A.

 

From: Urdiansyah

Sent: Δευτέρα, 19 Οκτωβρίου 2015 - 07:42

To: Materials & Welding

Subject: [MW:23742] MT before or after PWHT?

 

Dear Expert,

 

Currently I work at fabricator of Pressure vessel and Heat exchanger,

During Renewal ASME, AI question about MT shall be done before or after PWHT ?

Kindly  advice for this matter

 

Thank you for answered,

 

Best Regards,

Urdiansyah

Engineering PIC

PT.Daekyung Indah Heavy Industry

Cilegon Plant :

Jl. Australia II Kav. K1 Kawasan Industri (KIEC)

Cilegon 42443, Banten - INDONESIA 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4c4f5ad7-fc11-4d20-a7c3-0ac84044a3b2%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/OF0D8BA562.4CB7F0F0-ONC1257EE3.00506273-1445265481162%40LocalDomain.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/B1C5C970BEA29243935FA5EB72F113C80208ECFF3B%40BOLEXVSG11.chaco.com.bo.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...