Dear Sir/Experts,
We are going to the manufacturing the Sphere for Liquid/unsaturated LPG.Design Code ASME Section -Vlll Div-2, design temperature -34 deg centigrade. Materials are impacted tested at  -34 deg centigrade wıth simulated heat treatment. condition.
I have doubt regarding PTC. As per Section Vlll Div-1 if materials are under impact tested in that case PTC is mandatory. 
But as per ASME Section Vlll Div-2 it is required or not please advised me with supporting clause/documents.


--
Thanks & Regards
Pinaki Boxi.
*Manager QA/QC*
*ARP Project Site, Turkey*
*Mob :- +905351054384.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOt02TCwCpbYde3uSevpac%3D8m-HSVO4MdP62%3DQ8D7nvHp6Tnhg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...