[MW:23782] Weld Repair Procedure as per API 1104

Dear Members,

We qualified Welding Procedure on API 1104, now our Client is demanding Weld Repair Procedure Qualification.
In scope Weld Repair Procedure Qualification is not mentioned.
I need expert judgement that is it mandatory to qualify Weld Repair Procedure for each welding procedure in API 1104.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKhANKhXe8wcUM8B4nReA8KTi%3DQAW%3DyQBZMdSz%2BToYK3hgpiyA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...