Tuesday, October 20, 2015

Re: [MW:23758] Materials Comparison Form

Mr Boxi,

You have to satisfy AI that re certification is meeting requirements of construction Code viz UG-10(a) (2) of ASME SecVIII-I 

On the other hand compare requirements mentioned in ASTM A537 & SA537 for Melting Method, Melting practice, Manufacturing's process, De oxidation; if all are same for both standard then we can justify meeting SA537-2013 as well
 
Regards

Aly

On Sun, Oct 18, 2015 at 10:12 AM, Perumal Govindan <perumalgovindan@gmail.com> wrote:
Mr Boxi,

Ok, request NISCO to provide COC (after referring the MR/PR/PO about material spec and grade requirement), sample COC was attached (from other manufacturer) for your information.

Please ensure the below points to be indicated on the COC:

1. Material Specification as per ASME Section II Part A: 2013 shall be ASME SA 537 / SA 537 Class 1


4. Manufacturing Process and material condition
4.1 Steelmaking Practice — The steel shall be killed
and conform to the fine austenitic grain size requirement
of Specification A 20/A 20M.

 5. Heat Treatment
5.1 All plates shall be thermally treated as follows:
5.1.1 Class 1 plates shall be normalized.
5.1.2 Class 2 and Class 3 plates shall be quenched
and tempered. The tempering temperature for Class 2 plates
shall not be less than 1100°F [595°C] and not less than
1150°F [620°C] for Class 3 plates.

6. Chemical Requirements (ask also to indicate Ceq. compliance)
6.1 The steel shall conform to the chemical requirements
shown in Table 1 unless otherwise modified in accordance
with Supplementary Requirement S17, Vacuum
Carbon-Deoxidized Steel, in Specification A 20/A 20M.


Regards
P Govindan
L&T HCI-PQM,
Abu Dhabi.

On Sat, Oct 17, 2015 at 11:34 PM, Pinaki Boxi <boxi.pinaki@gmail.com> wrote:
Dear Mr. Govindan,
Right now MTC is not possible to change, please advice without change the MTC.

On 10/17/15, Perumal Govindan <perumalgovindan@gmail.com> wrote:
> Mr Boxi,
>
> Advise NISCO to replace all the MTCs as per ASME material specifaction.
>
> As a Contractor / Buyer you would have commented on the draft MTC before
> printing as a final copy. You would have atleast specified on PR and PO.
>
> Now only the option to replace the MTC, Client will not accept the
> deviations. Hence, disciss with NISCO for the new MTC as per ASME Section
> II.
>
> Regards
> P Govindan
> L&T HCI-PQM,
> Abu Dhabi.
> On 17 Oct 2015 12:47, "Pinaki Boxi" <boxi.pinaki@gmail.com> wrote:
>
>> Dear Sir/Expert,
>> As per Design requirements Sphere materials shall be ASME SA537 Cl.1
>> 2013Ed. but we received ASTM A537 Cl.1 2013Ed. materials at site.because
>> of
>> that client needs materials comparison Form and it shall be sing by AI
>> (Authorized İnspector )
>> As per AI, requirements Melting Method, Melting practice, Manufacturing's
>> process, De oxidation shall be in the Materials comparison Form.
>> But MTC mention only Fully Killed and Fine Grain Practice steel, Vacuum
>> Degassed.
>> So requested to please be advice how we get all the AI requirements from
>> MTC .
>> Materials Comparison Form & MTC attached for ready reference.
>>
>> --
>> Thanks & Regards
>> Pinaki Boxi.
>> *Manager QA/QC*
>> *ARP Project Site, Turkey*
>> *Mob :- +905351054384.
>>
>> --
>> You received this message because you are subscribed to the Google Groups
>> "Materials & Welding" group.
>> To unsubscribe from this group and stop receiving emails from it, send an
>> email to materials-welding+unsubscribe@googlegroups.com.
>> To post to this group, send email to materials-welding@googlegroups.com.
>> Visit this group at http://groups.google.com/group/materials-welding.
>> To view this discussion on the web visit
>> https://groups.google.com/d/msgid/materials-welding/CAOt02TCyda1PRG2iFj-FORe%3DZaD0Y_Qzah80semHyWxcnM6fQQ%40mail.gmail.com
>> <https://groups.google.com/d/msgid/materials-welding/CAOt02TCyda1PRG2iFj-FORe%3DZaD0Y_Qzah80semHyWxcnM6fQQ%40mail.gmail.com?utm_medium=email&utm_source=footer>
>> .
>> For more options, visit https://groups.google.com/d/optout.
>>
>
> --
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com.
> To post to this group, send email to materials-welding@googlegroups.com.
> Visit this group at http://groups.google.com/group/materials-welding.
> To view this discussion on the web visit
> https://groups.google.com/d/msgid/materials-welding/CANiuf9ebY%3DgZXOh_bmb4UYfYpOHirWNq1JWimxymXt4qAG_HVg%40mail.gmail.com.
> For more options, visit https://groups.google.com/d/optout.
>


--
Thanks & Regards
Pinaki Boxi.
*Manager QA/QC*
*ARP Project Site, Turkey*
*Mob :- +905351054384.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOt02TDS-zADEKZan7x-NcDia7rSr%3Dety9FTOk134vCpxYksFw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.




--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANiuf9cLOuivgxx6XOpYwObfo7J2AfOrTCKNxHLddyMztDQgwQ%40mail.gmail.com.

For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOenW4jzgpd2rDf48PnHvohmfFzcwxWjprU9SpYk8uKK5eRe_A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...