Skip to main content

Re: [MW:23748] Impact Test Requirement for Welds of API-650 Storage Tank when Design Metal Temperature is below -7°C

Dear

ASME SECIX is only a qualification code.Impact test requirements is out of the scope of SECIX.It is design code or client specification which specify impact test requirements as per service conditions.

Regards,
Mohammed Azharuddin

--------------------------------------------
On Sun, 18/10/15, Vanchinath S.A. <vanchinaths@gmail.com> wrote:

Subject: Re: [MW:23739] Impact Test Requirement for Welds of API-650 Storage Tank when Design Metal Temperature is below -7°C
To: materials-welding@googlegroups.com
Date: Sunday, 18 October, 2015, 8:57 AM

Design code
to be followed for impact test requirements. Follow API
650.


On 17 Oct 2015 13:27,
"SA" <sarfrazengineer@gmail.com>
wrote:
Dear All,
A Fuel
Oil tank has been designed as per API-650 code and it is
mentioned in this code that when design metal temperature is
below -7°C impact test shall be carried out for all welds
for all components. The statement in code is given
as: 
"9.2.2.2
When the design metal temperature is below -7°C (20 OF),
impact tests of the weld metal shall be made for all
procedures used for welding the components listed in 4 2.10
1, for welding attachments to these components, and for
fabricating shell nozzles and manholes from pipe and
forgings listed in 4.5. 
In our case, design metal
temperature is below -7°C i.e. -10°C but still welding
engineer is insisting that impact testing is not required as
per ASME Section IX (QW-403.5).
My question is that Tank is designed
as per API-650 and there is no reference that ASME section
IX would supersede  the above statement of API-650 where
impact testing shall be carried out when Design Metal
Temperature is below -7°C.
Can anybody guide on this
subject.
Thanks in
advance



--

You received this message because you are subscribed to the
Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails
from it, send an email to materials-welding+unsubscribe@googlegroups.com.

To post to this group, send email to materials-welding@googlegroups.com.

Visit this group at http://groups.google.com/group/materials-welding.

To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b751b08a-e0c5-4b0d-8b76-34555fc91bcd%40googlegroups.com.

For more options, visit https://groups.google.com/d/optout.





--

You received this message because you are subscribed to the
Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails
from it, send an email to materials-welding+unsubscribe@googlegroups.com.

To post to this group, send email to materials-welding@googlegroups.com.

Visit this group at http://groups.google.com/group/materials-welding.

To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2B6Tn1%2BN-WtZEryA90%2BS1nV%3DrJB73FkSP0yfXJTtM86go33ZUQ%40mail.gmail.com.

For more options, visit https://groups.google.com/d/optout.


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1445262134.54053.YahooMailBasic%40web193205.mail.sg3.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...