[MW:23633] PWHT as per latest 31.3 (2014)

All,

If we refer to ASME B 31.3 latest issued (2014), the Table 331.1.3 (Exemption to Mandatory Postweld Heat Treatment), the tabulation for P 1 (all groups), it indicated that "All thicknesses" for "All of type of welds" there is no need to perform PWHT. Except that >25mm they need to perform preheat at 95degC.



So based on above, it now looks all thicknesses are exempted from PWHT, and there is no need to even perform preheat for weld thicknesses <=25mm; and if we just perform preheat the PWHT is now exempted for any thicknesses. Table 330.1.1 -2014 indicated Preheat for <=25mm is 10degC (again it is not clear on this 10degC requirement).



Whereas, B 31.4, B31.8, ASME Sec VIII Ć  all these 3 codes indicate that PWHT is mandatory for thickness >1.5", and preheat mandatory for weld thickness >1.25" for all P1 materials.



So, we have to be clear as many of our Operation / Maintenance / PMT are in need of a clear understanding of the B31.3-2014 requirements on PWHT.



B 31.3 – 2014 – my understanding (based on para 331.1.1(a), (b), (c) is PWHT can be exempted, provided the WPS/PQR is qualified (without preheat for less <=25mm, and with preheat for thickness >25mm). The PQR qualification tests shall be as per ASME Sec IX as minimum (and any extra ex: Impact testing if low temperatures, hardness test if NACE etc).



Assuming that the PQR tests pass (without the coupon undergoing PWHT for any thickness in P1), now the code B 31.3 is giving exemption to PWHT.



And if any of the required tests during PQR fail, then the fabricator to re-perform this PQR with PWHT, and re-test to ensure that all test results pass.


(otherwise I do not see any reason, how Code B 31.3-2014 has given this blank concession for all thicknesses, as preheat >25mm or no preheat for <=25mm does not guarantee that PQR test results will pass).

Get your own FREE website, FREE domain & FREE mobile app with Company email.  
Know More >

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1443670500.S.20040.autosave.drafts.1443670541.26663%40webmail.rediffmail.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...