Dear Mr. Poojary,

QW-202.2(c) says:
''Qualification for Fillet Welds. WPS qualification for fillet welds may be made on groove-weld test coupons using test specimens specified in (a) or (b). Fillet-weld procedures so qualified may be used for welding all thicknesses of base metal for all sizes of fillet welds, and all diameters of pipe or tube in accordance with Table QW-451.4. Nonpressure-retaining fillet welds, as defined in other Seetions of the Code, may as an alternate be qualified with fillet welds only. Tests shall be made in accordance
with QW-180. Limits of qualification shall be in accordance witb Table QW-451.3.''

Table QW-451.4 Fillet Welds Qualified by Groove-Weld Tests shall also be considered.

Best regards

Parvan Chavdarov

Dr.-Ing. Parvan Chavdarov
ASME A, B & N Inspector,IWE
Business Unit Nuclear Safety

TÜV Rheinland Industrie Service GmbH
Am GrauenStein
51105 Köln
Tel.: + 49 221 806 4251
Fax: + 49 221 806-3402
Mobile: + 49 151 53171362
parvan.chavdarov@de.tuv.com

----- Цитат от Jay Poojary (jayogini@gmail.com), на 28.09.2015 в 17:18 -----

Dear Experts,
 
As per ASME, Welder is qualified to weld fillet joint, if he is qualified on groove joint. My question is -------------

 Wps approved for groove joint is applicable for fillet joint?

  If so where it is stated.

cordially,
Jay Poojary

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAcO%3DySZQkp22fraccZK2Eohv1k-CisD_Z2_p7XssaRAf9YEaw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



Dr.-Ing. Parvan Chavdarov



ASME A, B & N Inspector, IWE



Business Unit Nuclear Safety



 



TÜV Rheinland Industrie Service GmbH



Am Grauen Stein



51105 Köln



Tel.: + 49 221 806 4251



Fax: + 49 221 806-3402



Mobile: + 49 151 53171362



parvan.chavdarov@de.tuv.com



-------------------------------------
Mail.BG: Безплатен e-mail адрес. Най-добрите характеристики на българския пазар - 20 GB пощенска кутия, 1 GB прикрепен файл, безплатен POP3, мобилна версия, SMS известяване и други.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da02beb08b6ab2a70f0154fd0c5967d6.mailbg%40mail.bg.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...