Saturday, September 26, 2015

[MW:23563] Re: Qualified WPS On AWS D1.4

Dear Mostafa
Pl. don't send mails to individuals. Shooting off an e-mail to a person which you are not familiar will most likely be ignored. sending to the group ID in anyway will reach everyone in the forum

Thank you!

On Saturday, September 26, 2015 at 8:48:18 PM UTC+5:30, Mostafa Kamel Hussein wrote:
Dear All,
Has any body qualified WPS based on AWS D1.4 to cover welds on pile cages as it was carried out in my site? the owner requested a qualified WPS to close this issue?
Your prompt action is highly appreciated.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7d12aa0a-33a5-4ca4-b3a0-b00057aca35c%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...