[MW:23575] Regarding RT before or after PWHT

Dear Sir,

As we all aware that PWHT and RT both are different in nature, in general we perform RT after PWHT(Where PWHT is required to be perform after welding). 

However it is not written anywhere that RT is to be performed after PWHT only.

My question now is , can we perform RT first and then go for PWHT? will it be acceptable ????.
I have seen many client inspectors asked contractors to perform PWHT first then RT whereas their specifications does not say anything in this regard.

All experts are requested to throw light on the subject. Documented proof/literature , if any, to support this will be higly appreciable.



regards,

Ajay 


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM6T1-EGdHb%3DKoxGb-OuLZr5Dr8KpP7_dLG72WQ6AaUdJ-XG-w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...