I don't suggest you a coating, otherwise you can use Carbon Steel Coated. A better procedure is to clean the surface with sandblasting with a finishing step applying a degreasing solution.

I agree with other answers: probably this is due to contamination to carbon steel (maybe come from grinding powders) or pitting corrosion due to a high corrosive environment. In this last case I suggest you to change Material with Carbon Steel galvanized.

Regards

Il giorno martedì 29 settembre 2015 09:00:50 UTC+2, neilash kumar ha scritto:
Dear Sir,

Good Morning, please find the attached tank drawing
 fabricated by us for our client & it is corroded fully ,
Can you please clarify,
 1. Why the tank are corroded So fast?
 2. Can you please advise us the method to stop /reduce the rate of corrosion by applying a top coat &  what
type of coating to be applied?

please advise me . Material is 316L tank.
 
Regards
P.Neilashkumar

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ba743560-4c96-417f-9781-4a67a7d1b0b2%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...