Re: [MW:23614] Re: NEED ADVISE CORROSION IN INHIBITOR TANK REGD

Pickling will remove any oxides from welds but if you are finishing the welds and removing the chromium oxide then passivation would suffice as it will remove any carbon traces that remain. We use a high nitric content for passivation that is considered a light pickling. We use this on 300 series Stainless and 2101 and 2205 Duplex material.

Best Regards,

Jim Price 

Sent from my iPad
Picking would remove contaminants (iron)

Sent from my BlackBerry 10 smartphone.
From: Neilashkumar
Sent: Τρίτη, 29 Σεπτεμβρίου 2015 - 19:14
To: George H Dilintas
Cc: Welding Groups
Subject: Re: NEED ADVISE CORROSION IN INHIBITOR TANK REGD

Dear sir ,

Thanks for your answer , now I have doubt instead of pickling spray can I go directly to passivation spray followed by rinsing and cleaning. I need your advise and procedures if any?

P.NEILASHKUMAR 
Sent from my iPad
MOB : 966 533098265
            91+9952110791

On Sep 29, 2015, at 10:04 AM, george.dilintas@gr.bureauveritas.com wrote:

It looks like iron contamination.
Actions to implement:

  1. Removal of rust by stainless steel compatible brushes/disks.
  2. Pickling
  3. Avoid contact with carbon steel tools, jigs etc

best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04


Neilash Kumar ---29/09/2015 09:56:39--- Dear Sir, Good Morning, please find the attached tank drawing

From: Neilash Kumar <neilashkumar@yahoo.com>
To: George H Dilintas/GRC/VERITAS@VERITAS, Welding Groups <materials-welding@googlegroups.com>
Date: 29/09/2015 09:56
Subject: NEED ADVISE CORROSION IN INHIBITOR TANK REGD




 Dear Sir,

Good Morning, please find the attached tank drawing
fabricated by us for our client & it is corroded fully ,
Can you please clarify,
1. Why the tank are corroded So fast?
2. Can you please advise us the method to stop /reduce the rate of corrosion by applying a top coat &  what
type of coating to be applied?

please advise me . Material is 316L tank.

Regards
P.Neilashkumar[attachment "20150909_102338.jpg" deleted by George H Dilintas/GRC/VERITAS] [attachment "20150909_102358.jpg" deleted by George H Dilintas/GRC/VERITAS]

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/OF57240EB1.3777AADA-ONC1257ECF.005C9F78-1443545501800%40LocalDomain.
For more options, visit https://groups.google.com/d/optout.