ASME Section IX QW303.2 and QW461.9 gives you the positions qualified for
Best Regards
Jim Price | Welding Engineer, CWI
Direct: 320.7463439 | Fax: 417-862-5564
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Jay Poojary
Sent: Monday, September 28, 2015 10:18 AM
To: materials-welding@googlegroups.com
Subject: [MW:23577] Fillet weld
Dear Experts,
As per ASME, Welder is qualified to weld fillet joint, if he is qualified on groove joint. My question is -------------
Wps approved for groove joint is applicable for fillet joint?
If so where it is stated.
cordially,
Jay Poojary
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAcO%3DySZQkp22fraccZK2Eohv1k-CisD_Z2_p7XssaRAf9YEaw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Comments