Wednesday, September 30, 2015

Re: [MW:23614] RE: 23575] Regarding RT before or after PWHT

Yes P15E very much.

On 29-Sep-2015 9:58 pm, <george.dilintas@gr.bureauveritas.com> wrote:
P-No 15E included. Example P91. For the other Pnos the Engineering has to agree for the PWHT timing. Check closer in B31.1

Sent from my BlackBerry 10 smartphone.
From: Kannayeram Gnanapandithan
Sent: Τρίτη, 29 Σεπτεμβρίου 2015 - 16:47
To: materials-welding
Subject: Re: [MW:23605] RE: 23575] Regarding RT before or after PWHT

ref B31.1, 136.4, NDE of P3,4 &5A and 5B materials welds shall be performed after PWHT. For other materials , NDE may be before or after PWHT

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY

On Tue, Sep 29, 2015 at 1:40 PM, Ajay <donsaab3@gmail.com> wrote:
Dear Sir,

I do agree with u completely,,,,,,,,,,,,But many contractors adament to do RT after PWHT.......if any documents to support the statement would be highly appreciated.

On Tue, Sep 29, 2015 at 1:33 PM, Alan Denney <alan@denney1.freeserve.co.uk> wrote:

NDT for final acceptance will be after PWHT. However it is relatively common to perform intermediate (in-house) NDT and perform any repairs prior to PWHT.

PWHT will relieve residual stress and can open up flaws which are otherwise closed by the residual stresses, and that is the reason why NDT for acceptance purposes is performed after PWHT.

 

Alan Denney

AKD Materials Consulting Ltd

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Ajay
Sent: 29 September 2015 05:03
To: materials-welding@googlegroups.com
Subject: [MW:23575] Regarding RT before or after PWHT

 

Dear Sir,

 

As we all aware that PWHT and RT both are different in nature, in general we perform RT after PWHT(Where PWHT is required to be perform after welding). 

 

However it is not written anywhere that RT is to be performed after PWHT only.

 

My question now is , can we perform RT first and then go for PWHT? will it be acceptable ????.

I have seen many client inspectors asked contractors to perform PWHT first then RT whereas their specifications does not say anything in this regard.

 

All experts are requested to throw light on the subject. Documented proof/literature , if any, to support this will be higly appreciable.

 

 

 

regards,

 

Ajay 

 

 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM6T1-EGdHb%3DKoxGb-OuLZr5Dr8KpP7_dLG72WQ6AaUdJ-XG-w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


This email has been scanned by BullGuard antivirus protection.
For more info visit www.bullguard.com

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/004101d0fa8d%245f012e30%241d038a90%24%40denney1.freeserve.co.uk.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM6T1-F-ZVH%3DT6iweXK0etBbsiNr%3DvTt-1%2Bhu%2BYAfC%3DXin1UYw%40mail.gmail.com.

For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePp43i7ks%2BqKtkdFXo3cXDJw-77i5KGTk1xxWyTjR%2B85Q%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/OFB4537794.0A439131-ONC1257ECF.0052ACE2-1443538982310%40LocalDomain.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNh2EWVyThGSf279S%3Db5q3zeoAPAYRUU5MMMqwXYbkEaA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...