Tuesday, September 29, 2015

Re: [MW:23579] Regarding RT before or after PWHT

depends on 
1. Project specific requirements
2. MOC
3. Code of Construction

Generally NDE after PWHT is a project specific requirements, and not by code of construction (except few materials, e.g. UHA 33(b) for ASME BPV div 1 vessels, or para 341.3.1.(a) for ASME B31.3 process piping welds)

On 29 September 2015 at 08:03, Ajay <donsaab3@gmail.com> wrote:
Dear Sir,

As we all aware that PWHT and RT both are different in nature, in general we perform RT after PWHT(Where PWHT is required to be perform after welding). 

However it is not written anywhere that RT is to be performed after PWHT only.

My question now is , can we perform RT first and then go for PWHT? will it be acceptable ????.
I have seen many client inspectors asked contractors to perform PWHT first then RT whereas their specifications does not say anything in this regard.

All experts are requested to throw light on the subject. Documented proof/literature , if any, to support this will be higly appreciable.



regards,

Ajay 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVub%3DvtU9mUvVjp54GjHUjowXCa3do0W6kyeKv-7DAVfEn%2BQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...