[MW:20848] Re: Fw: Difference between A671 & A672

I am quite later to reply this.

The difference lies in the testing requirements. A672 requires weld sample drawn from 500ft length of pipe and allows you to double the samples in case, original sample fails. A671 requires weld sample drawn from 200ft length of pipe with no provision for rejected weld.

On Monday, November 15, 2010 10:09:10 AM UTC-7, Dhwani Desai wrote:

Dear Members,

In general, we all know based on description given in ASTM of A671 & A672 that A671 is used for atm. & low temperature service & A672 for H.P. service at moderate temperature.

However, if we compare the details e.g. A672 Gr.C60  & A671 Gr. CC60; the raw material plate used is same for both pipes & final mechanical properties is same.
Heat treatment is same.
Can any one explain or comment if  A672 Gr.C60 with Suppl. req.S2 can be used for Low temp. service & why?


Dhwani Desai
Planning & Piping Dept.
Ext.-7681

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...